Sun-Lu PETG - 240C/90C - two perimeters - 30% infill, no elephant compensation so brim keeps it adhered nicely.  Printed in an enclosure.  Zero lift from build plate during or after print.  Brim and body are fully adhered.  I let it cool on my PEI sheet and once I remove it, it has this warp to it.  Bottom and walls are 7mm thick or so.

How can I print this so this warping does not occur?

MK3s / My IKEA Lack enclosure

Posted : 16/12/2020 7:56 pm
Swiss_Cheese
(@swiss_cheese)
Noble Member
RE: Warp after removal from plate - PETG - 215mm long print

sometimes people try to remove the prints from the bed before they have cooled completely, if the print went great and it didn't warp at all and the print completed, then try waiting until the print has completely cooled, even waiting beyond the time it takes for the bed to cool down. this isn't a guarantee, it's a best practice.