Hello,

I've been noticing underextrusions with eSun eLastic filament in direct relation to the vertical height of the part. Increasing the extrusion multiplier leads to overextrusion on the first 4-7 layers, then adequate extrusion for the layers 7 - 12, then underextrusion  12-15. 

Is there another way to compensate for the under extrusion by having a overextrusion factor linked to the height of the layer?

Posted : 22/11/2021 8:31 pm
Dan Rogers
(@dan-rogers)
Noble Member
More likely there is a temperature issue

what temp are you trying to print your TPU at?  It's more likely that your temp is close to failure point (too cold) and as the print gets too tall the added boost from the bed has faded away.